Submicron Violet Tungsten Oxide

        Submicron violet tungsten oxide may be used to prepare submicron tungsten powder (W powder).

        Cyclic Oxidation-reduction Method to Produce Submicron Tungsten Powder
        Step one: First reduction of violet tungsten oxide in hydrogen (H2), when temperature reached 860°C, keep it warm for 20min.
        Step two: Use tungsten powder obtained in step one, slowly heat it to 500°C in air, process the first oxidation when temperature reaches 500°C, and then keep it warm for 10min.
        Step three: Use sample of step two and adopt process conditions in step one and step two, do the cyclic oxidation-reduction experiment to obtain W powder.
        Step four: Samples of the above steps were analyzed by using AR alcohol, and then the particle size and morphology of samples were analyzed by BT-9300 laser particle size analyzer and JXA-840A electron probe scanner respectively.submicron tungsten powder produced by submicron violet tungsten oxide picture
        Compared with current methods for preparing submicron tungsten powder at home and abroad, the W powder produced by using violet tungsten oxide and cyclic oxidation-reduction method has the advantages of simple equipment and process, and easy control of process parameters.

        More details, please visit:
        http://www.tungsten-powder.com/violet-tungsten-oxide.html

        Comments are closed.

        Address: 3F, No.25-1 WH Rd., Xiamen Software Park Ⅱ, FJ 361008,China Copyright ? 1997 - 2026 CTIA All Rights Reserved
        Phone:+86-592-5129696,+86-592-5129595;    Email: [email protected]
        舊版

              东京热AV无码国产东京热AⅤ | 99热官方网站 | 日韩视频中文 | 天堂网av2018 | 无码人妻一区二区三区免费n狂飙 | 伊人草大香蕉 | 天天影视网色欲 | 麻豆精品在线影院 | 色播在线永久免费视频 | 大屌逼视频 |