Arsenic Doped Ammonium Metatungstate Preparing Nano Tungsten Powder

        Arsenic doped ammonium metatungstate (AMT) is generated by adding ammonium metatungstate into the nitric acid solution of elemental arsenic and stirring, drying and grinding, the excellent raw material for preparing nano tungsten powder. Nano tungsten powder is the tungsten powder which the particle size is fine to nanoscale, at present, the traditional method for manufacturing nano tungsten powder is tungsten oxide reduction method, wherein the reducing agent maybe hydrogen or carbon; with the appearing of nano materials, the manufacture methods of nano tungsten powder are emerging constantly, such as high-energy ball milling, gas evaporation, plasma, self-propagating high-temperature reduction and molten salt electrolysis method.

        There is a study to take ammonium metatungstate as raw material, and through doping process to get arsenic doped ammonium metatungstate to finally get nano tungsten powder, with the producing process like the following:
        1. Preparation of arsenic doped ammonium metatungstate precursor composite powder
        Add a certain amount of elemental arsenic into the nitric acid with a certain concentration, then add ammonium metatungstate into the nitric acid solution of elemental arsenic after the As is completely dissolved with the arsenic content being controlled; electric mix the raw materials, then dry them in a oven under 70~90°C for 8~10 hours, and then, grind to get arsenic doped ammonium metatungstate precursor compound powder.
        2. Arsenic doped ammonium metatungstate calcination to prepare yellow tungsten trioxide powder
        Put the prepared arsenic doped ammonium metatungstate precursor compound powder in a box type resistance furnace at the temperature of 580~620°C to carry out calcination in air atmosphere for 2~3 hours, then we get yellow tungsten trioxide powder.
        3. Tungsten trioxide reduction to generate nano tungsten powder
        Put the yellow tungsten trioxide powder in a tube furnace to get reduction by inletting hydrogen, under the reduction temperature of 780~820°C with the heating rate of 5°C/min, and the heat preservation time of 3~4 hours, to finally manufacture nano tungsten powder

        The nano tungsten powder get by arsenic doped ammonium metatungstate has the advantages of good dispersion, and uniform particle size distribution, thus to effectively promote the development and application of nano-crystal WC-Co alloy.

        Comments are closed.

        Address: 3F, No.25-1 WH Rd., Xiamen Software Park Ⅱ, FJ 361008,China Copyright ? 1997 - 2026 CTIA All Rights Reserved
        Phone:+86-592-5129696,+86-592-5129595;    Email: [email protected]
        舊版

              粉嫩视频在线播放 | 婷婷五月天AV | 国产做受 91电影 | 免费直接观看的黄色 | 国产成人精品777777 | 午夜精品久久久久久久99黑人 | 国产一级婬乱A片 | 成人精品毛片 | 外国女人操逼在线视频 | 中文字幕成人在线播放 |