How to Prepare Tungsten Disulfide Nanosheet?

        How to prepare tungsten disulfide nanosheet? There are common methods for preparing nano tungsten disulfide at present, such as direct pyrolysis and chemical vapor deposition. However, these methods require the conditions of high temperature and vacuum, and the process is complicated. In this regard, the researchers proposed a preparation method of WS2 nanosheets that can be carried out at low temperature, with a simple process flow and little pollution.

        More details, please visit:
        http://tungsten-disulfide.com/index.html

        how to prepare tungsten disulfide nanosheet? image

        Preparing Tungsten Disulfide Nanosheets by Solvothermal Method
        Add a certain amount of Li2CO3 powder, WS2 powder and 40mL of organic solvent benzyl alcohol solution to high-pressure reaction kettle with a volume of 50mL, and place the high-pressure reaction kettle at a temperature of 200 °C for 48 h for solvothermal reaction. Wash the reaction product with deionized water, acetone, and absolute ethanol, vacuum-dried and collected, and the obtained product was added to a mixed solution of deionized water and NN-dimethylformamide in a volume ratio of 1:1, followed by continuous ultrasonic vibration for 12 h. The solution was centrifuged at 600 r/min for 30 min, the supernatant was taken, and the clear was centrifuged at 6000 r/min for 10 min to collect the precipitate. And then wash the precipitate with 3% HCl, deionized water, and absolute ethanol, vacuum dried to collect WS2 nanosheets.

        Comments are closed.

        Address: 3F, No.25-1 WH Rd., Xiamen Software Park Ⅱ, FJ 361008,China Copyright ? 1997 - 2026 CTIA All Rights Reserved
        Phone:+86-592-5129696,+86-592-5129595;    Email: [email protected]
        舊版

              黄色国产视频在线观看 | 欧美黑人一级A片免费看 | 婷婷色视频在线观看 | 午夜久久久久久久 | 在线天堂8 | 久操精品| 亚洲欧洲欧美日韩中文字幕 | 美女喷水网站 | 黄色一级片A | 五月天激情综合网 |